XXXVIII IULTCS Congress · 2025 · L-O-024
Marcelo Bertazzo; Alex Migallón; Margarita Rodríguez Álvarez; Elena Orgilés Calpena
Abstract matchFull-text match
… in which biodegradation is determined by quantifying the CO ₂ produced during collagen degradation. This is achieved through direct infrared detection and continuous CO ₂ concentration …
Open original PDF →XXXVIII IULTCS Congress · 2025 · L-O-006
Francina Izquierdo; Ivo Reetz; Anna Bacardit
Abstract matchFull-text match
… the pretanned/tanned leathers was assessed using ISO 20136, revealing a 94% degradation rate compared to non-tanned collagen—considerably higher than that achieved with conventional tanning methods. Additionally, compostability, as …
Open original PDF →XXXVII IULTCS Congress · 2023 · P-0299
Chunqiong Li; Haojie Qin; Xiaojun Shen
Abstract matchFull-text match
… show that the tannability of leather can be improved by combining disaldehyde -degradation products with titanyl sulfate.The shrinkage temperature of DAS combined with titanium oxide sulfate increased by 9℃ compared with that of DAS alone . The dispersi on and fixation degree of collagen fiber network of leather tanned by the combination of degraded DAS and …
Open original PDF →13th AICLST Congress · 2026 · TI-49-O
Anusuya Annamalai, N Nishad Fathima1*
Abstract matchFull-text match
… GS powder) to achieve enhanced hydrothermal stability, durability, and resistance to environmental degradation as an alternative approach to Chrome tanning. Vegetable tannin reinforces crosslinking through hydrogen bonding and hydrophobic interactions while phenolic ligand phloroglucinol enables chelation with Al³z , improving its affinity toward carboxyl and amine groups in collagen. FT-IR and MALDI-TOF characterisation techniques confirm the formation of PHO-AL. Hydrothermal shrinkage …
Open original PDF →XXXVIII IULTCS Congress · 2025 · L-O-023
Volker Rabe; Jens Fennen; Biju Francis; Florian Doeppert
Abstract matchFull-text match
… stabilizing but less degradable systems reduce compostability. Additives with little or no collagen interaction, such as fillers and polymers, showed only minor influence on degradation rates. Overall, the results highlight the importance of selecting appropriate retanning systems …
Open original PDF →III IULTCS EuroCongress · 2022 · V-O-112
Anke Mondschein1, Michaela Schröpfer1, Michael Meyer1
Full-text match
… resources in leather production. During the production of leather from hide, the collagen is chemically crosslinked to stabilize it thermally and against enzymatic degradation by microorganisms. The hides are usually washed, dehaired and pre-tanned. These pre-tanned …
Open original PDF →13th AICLST Congress · 2026 · TI-109-O
Nayan Ranjan Singha a,b and Pijush Kanti Chattopadhyay a,b
Full-text match
… Li, C. Preparation of Mesoporous TiO2 and Pt- Doped TiO2 Fibers with Collagen Fiber as a Template and Their Performance for Photocatalytic Degradation of Black Liquor. J. Chin. Ceram. Soc., 2012, 40, 1489–1494. 21 …
Open original PDF →XXXVII IULTCS Congress · 2023 · P-10-103
Zhiwei Chen; Ruxin Zhang; Deyi Zhu
Full-text match
… The influences of 3, 4 -dihydroxybenzaldehyde on the microstructure and stability of collagen fibrils, Polymer Degradation and Stability, 161, 198- 205, 2019. [23] Huo Q.Q., et al …
Open original PDF →XXXVIII IULTCS Congress · 2025 · L-O-002
Yang (John) Liu; Yash Dixit; Siew Ling Ong; Sujay Prabakar; Marlon M. Reis
Full-text match
… skins —by-products of the meat industry —into durable goods by stabilising the collagen matrix and preventing microbial degradation (Zhang et al., 2018). However, raw hides are vulnerable to microbial spoilage …
Open original PDF →13th AICLST Congress · 2026 · TI-47-P
Guanjie Huanga, Jianzhong Mab, Jie Chenc
Abstract matchFull-text match
… loosely organized structure with enhanced crosslinking efficiency. The chemical stability of modified collagen fibers was analyzed through enzyme degradation experiments. As shown in Figure 2h, the residual mass of pickled skin …
Open original PDF →